| Code |
Title |
| GB/T 147–1997 |
Writing paper and certain classes printed matter-Untrimmed sizes |
| GB/T 148–1997 |
Writing paper and certain classes printed matter-Trimmed sizes-A and B series |
| GB/T 450–2002 |
Paper and board – Sampling for testing |
| GB/T 451.1–2002 |
Paper and board – Determination of size and deviation |
| GB/T 451.2–2002 |
Paper and board – Determination of grammage |
| GB/T 451.3–2002 |
Paper and board – Determination of thickness |
| GB/T 452.1–2002 |
Paper and board identification of machine and cross direction |
| GB/T 452.2–2002 |
Paper and board identification of wire side and felt side |
| GB/T 453–2002 |
Paper and board – Determination of tensile properties (Constant rate of loading methods) |
| GB/T 454–2002 |
Paper determination of bursting strength |
| GB/T 455–2002 |
Paper and board determination of tearing resistance |
| GB/T 456–2002 |
Paper and board – Determination of smoothness (Bekk method) |
| GB/T 457–2002 |
Paper – Determination of folding endurance (Schopper method) |
| GB/T 458–2002 |
Paper and board – Determination of air permeance (Schopper method) |
| GB/T 459–2002 |
Paper and board – Determination of dimensional instability |
| GB/T 460–2002 |
Paper – Determination of the sizing value (Ink line method) |
| GB/T 461.1–2002 |
Paper and board – Determination of capillary rise (Klemm method) |
| GB/T 461.2–2002 |
Paper and board – Determination of the rate of surface absorbing |
| GB/T 461.3-1989 |
Paper and board – Determination of absorption (after immersion in water) |
| GB/T 462-2003 |
Paper and board – Determination of moisture content |
| GB/T 464.1-1989 |
Paper and board accelerated ageing – dry heat treatment(105oC±2oC,72h |
| GB/T 464.2–1993 |
Paper and board– Accelerated ageing – dry heat treatment at 120 or 105oC |
| GB/T 465.1–1989 |
Paper and board – Determination of bursting strength after immersion in water |
| GB/T 465.2–1989 |
Paper and board – Determination of tensile strength after immersion in water |
| GB/T 740–2003 |
Pulps – Sampling for testing |
| GB/T 741–2003 |
Pulps – Determination of moisture content |
| GB/T 742–2003 |
Paper, board and pulp–Determination of residue(ash)on ignition at 900 |
| GB/T 743–2003 |
Pulps – Determination of ether solubles |
| GB/T 744–2004 |
Pulps–Determination of alkali resistance |
| GB/T 745–2003 |
Pulps – Determination of pentosan content |
| GB/T 747–2003 |
Pulps – Determination of acid-insoluble lignin |
| GB/T 1538–1979 |
Paperboard – Determination of folding endurance |
| GB/T 1539–1989 |
Paperboard – Determination of bursting strength |
| GB/T 1540–2002 |
Paper and board – Determination of water absorption – Cobb method |
| GB/T 1541–1989 |
Paper and board – Determination of dirt |
| GB/T 1543-1988 |
Paper – Determination of opacity (Paper backing) |
| GB/T 1545.1–2003 |
Paper, board and pulps – Determination of acidity or alkalinity of aqueous extracts |
| GB/T 1545.2–2003 |
Paper, board and pulps – Determination of pH of aqueous extracts |
| GB/T 1546-2004 |
Pulps – Determination of Kappa number |
| GB/T 1547-2004 |
Pulps – Determination of permanganate number |
| GB/T 1548-2004 |
Pulps – Determination of viscosity |
| GB/T 2677.1–1993 |
Fibrous raw material of sampling for analysis |
| GB/T 2677.2–1993 |
Fibrous raw material – Determination of moisture content |
| GB/T 2677.3–1993 |
Fibrous raw material – Determination of ash |
| GB/T 2677.4–1993 |
Fibrous raw material – Determination of water solubility |
| GB/T 2677.5–1993 |
Fibrous raw material – Determination of one percent sodium hydroxide solubility |
| GB/T 2677.6–1994 |
Fibrous raw material – Determination of solvent extractives |
| GB/T 2677.8–1994 |
Fibrous raw material – Determination of acid-insoluble lignin |
| GB/T 2677.9–1994 |
Fibrous raw material – Determination of pentosan |
| GB/T 2677.10-1995 |
Fibrous raw material – Determination of holocellulose |
| GB/T 2678.1–1993 |
Pulps – Determination of screened components |
| GB/T 2678.2–1994 |
Paper, board and pulps– Determination of water soluble chlorides (HgNO3 method) |
| GB/T 2678.3–1995 |
Pulps – Determination of chlorine consumption (Degree of delignification) |
| GB/T 2678.4–1994 |
Pulps and paper – Determination of zero-span tensile properties |
| GB/T 2678.5–1996 |
Paper, board and pulps – Determination of water soluble chlorides (AgNO3 method) |
| GB/T 2678.6–1996 |
Paper, board and pulps – Determination of water soluble sulphates (Conductimetric titration method) |
| GB/T 2679.1–1993 |
Paper – Determination of transparent |
| GB/T 2679.2–1995 |
Paper and board – Determination of water vapour transmission rate (Dish method) |
| GB/T 2679.3–1996 |
Paper and board – Determination of resistance to bending |
| GB/T 2679.4–1994 |
Paper and board – Determination of roughness (Bendtsen method) |
| GB/T 2679.5–1995 |
Paper and board – Determination of the folding endurance (MIT tester) |
| GB/T 2679.6–1996 |
Corrugating medium – Determination of the flat crush resistance after laboratory fluting |
| GB/T 2679.7-1981 |
Board – Determination of puncture resistance |
| GB/T 2679.8–1995 |
Paper and board – Determination of compressive strength – Ring crush method |
| GB/T 2679.9–1993 |
Paper and board – Determination of roughness (Print-surf method) |
| GB/T 2679.10-1993 |
Paper and board – Compressive strength – Short span test |
| GB/T 2679.11-1993 |
Paper and board – Qualitative analysis of mineral filler and mineral coating – SEM/EDAX method |
| GB/T 2679.12-1993 |
Paper and board – Qualitative analysis of mineral filler and mineral coating – Chemical method |
| GB/T 2679.13-1996 |
Paper and board – Determination of air permeance (medium range) – Bendtsen method |
| GB/T 2679.14-1996 |
Filter paper and filter board –Determination of maximum pore diameter |
| GB/T 2679.15-1997 |
Paper and board – Determination of printing surface strength – Accelerating speed method (electric model) |
| GB/T 2679.16-1997 |
Paper and board – Determination of printing surface strength – Accelerating speed method (pendulum or spring model) |
| GB/T 2679.17-1997 |
Corrugated fiberboard – Determination of edgewise crush resistance (Edge reinforced method) |
| GB/T 3332-2004 |
Determination of beating degree for pulps (Schopper – Riegler method) |
| GB/T 3333–1999 |
Cable paper – Determination of electrical strength at powerfrequence |
| GB/T 3334–1999 |
Method of test for dissipation factor (tgδ) of cable paper at power frequence (Schering bridge method) |
| GB/T 4687–1984 |
Paper, board and pulps terms – part 1 |
| GB/T 4688–2002 |
Paper, board and pulps – Analysis of fiber furnish |
| GB/T 5032–2002 |
Paper, board and pulps – Units for expressing properties |
| GB/T 5399-2004 |
Pulps – Determination of stock concentration |
| GB/T 5400–1998 |
Pulps – Method for determination of copper number |
| GB/T 5401–2004 |
Pulps – Determination of alkali solubility |
| GB/T 5402-2003 |
Paper and board – Determination of air permeance – Gurley method |
| GB/T 5405–2002 |
Paper – Determination of the sizing value (Liquid permeance method) |
| GB/T 5406–2002 |
Testing method of oil permeance for paper |
| GB/T 6545–1998 |
Corrugated fiberboard – Determination of bursting strength |
| GB/T 6546–1998 |
Corrugated fiberboard – Determination of edgewise crush resistance |
| GB/T 6547–1998 |
Corrugated fiberboard – Determination of thickness |
| GB/T 6548–1998 |
Corrugated fiberboard – Determination of ply adhesive strength |
| GB/T 7973–2003 |
Paper, board and pulps – Measurement of diffuse reflectance factor (Diff./0 – Geometry) |
| GB/T 7974–2002 |
Paper, board and pulps – Measurement of brightness (Diff/Geometry) |
| GB/T 7975–1987 |
Paper and board – Measurement of colour (Diffuse/o -geometry) |
| GB/T 7976-1987 |
Insulating paper and board – Determination of the electrical conductivity for the water extract |
| GB/T 7977–1987 |
Paper, board and Pulp – Determination of the electrical conductivity for the water extract |
| GB/T 7978–1987 |
Pulps – Determination of acid-insoluble ash |
| GB/T 7979-1987 |
Pulps – Determination of dichloromethance soluble matter |
| GB/T 8940.1-1988 |
Paper and board – Measurement of brightness (45/0) |
| GB/T 8940.2–2002 |
Pulps – Preparation of laboratory sheets for the measurement of brightness |
| GB/T 8941.1–1988 |
Paper and board – Measurement of specular gloss (20 degrees) |
| GB/T 8941.2–1988 |
Paper and board – Measurement of specular gloss (45 degrees) |
| GB/T 8941.3–1988 |
Paper and board – Measurement of specular gloss (75 degrees) |
| GB/T 8942–2002 |
Paper – Determination of softness |
| GB/T 8943.1-1988 |
Paper, board and pulp – Determination of copper content |
| GB/T 8943.2-1988 |
Paper, board and pulp – Determination of iron content |
| GB/T 8943.3-1988 |
Paper, board and pulp – Determination of manganese |
| GB/T 8943.4-1988 |
Paper, board and pulp – Determination of calcium and magnesium |
| GB/T 8944.1-1988 |
Pulps – Determination of saleable mass in lots part 1: Pulp baled in sheet form |
| GB/T 8944.2-1988 |
Pulps – Determination of saleable mass in lots part 2: (such as flash-dried pulp) baled in slabs |
| GB/T 10336–2002 |
Pulps – Determination of fiber length by automated optical analysis – Polarized light method |
| GB/T 10337–1989 |
Raw material and pulps – Determination of acid-soluble lignin |
| GB/T 10338–1989 |
Pulps – Determination of carboxyl content |
| GB/T 10339–1989 |
Testing method of light scattering and absorption coefficient for paper and pulps |
| GB/T 10340–1989 |
Paper and board – Determination of filtering rate |
| GB/T 10342–2002 |
Paper – Package and mark |
| GB/T 10739–2002 |
Paper, board and pulps – Standard atmosphere for conditioning and testing |
| GB/T 10740–2002 |
Pulps – Estimation of dirt and shives |
| GB/T 10741–1989 |
Pulps – Determination of alcohol – benzene solubles |
| GB/T 10742–1989 |
Raw fiber material – Determination of pectin content |
| GB/T 12032-1989 |
Paper and board – Preparation of a offset print for test gloss |
| GB/T 12033–1989 |
Determination of carbohydrate composition in raw materials and pulps by gas chromatograph |
| GB/T 12656–1990 |
Determination of electric strength at power frequency for capacitor paper |
| GB/T 12657–1990 |
Determination of conducting path for capacitor paper |
| GB/T 12658–1990 |
Paper, board and pulps – Determination of potassium and sodium content |
| GB/T 12659–1990 |
Pulps – Laboratory beating – Jokro mill method |
| GB/T 12660–1990 |
Pulps – Determination of drainability “Canada standard” freeness method |
| GB/T 12661–1990 |
Paper and board – Determination of microbiological properties – Total bacterial count |
| GB/T 12909–1991 |
Paper and board – Determination of bending stiffness – Resonance method |
| GB/T 12910–1991 |
Paper and board – Determination of titanium dioxide |
| GB/T 12911–1991 |
Paper and board – Determination of the ink absorbency |
| GB/T 12912–1991 |
Determination of separating capacity for chemical analysis filter paper |
| GB/T 12914–1991 |
Paper and board – Determination of tensile properties – Constant rate of elongation method |
| GB/T 13528–1992 |
Paper and board – Determination of surface pH |
| GB/T 14217–1993 |
Method of test for dielectric dissipation factor (tanδ) of capacitor paper at power frequence |
| GB/T 18402–2001 |
Pulps – Determination of drainability (drainage time method) |
| GB/T 18829.6–2002 |
Determination of fiber coarseness |
| QB/T 1461–1992 |
Air permeability of porous paper |
| QB/T 1462–1992 |
Pulps – Laboratory wet disintegration |
| QB/T 1463–1992 |
Pulps – Laboratory beating – PFI mill method |
| QB/T 1938–1994 |
Determination of thickness for soft paper |
| QB/T 2594–2003 |
Paper and board-Determination of surface strength (Wax method) |
| QB/T 2597–2003 |
Determination of fiber length for papermaking (raster method) |
| QB/T 2598–2003 |
Determination of fiber fibrillation for papermaking |
| QB/T 3533–1999 |
Polyester wire for papermaking – Test method |
| QB/T 3702–1999 |
Pulps – Laboratory beating – Valley beater method |
| QB/T 3703–1999 |
Pulps – Preparation of Laboratory sheets conventional sheet – former method |
| QB/T 3704–1999 |
Pulps – Laboratory sheets – Determination of physical properties |
| QB 1022–1991 |
General principles for calculation of total production |